silicon content in high Mn castings

Silicon: High silicon content reduces the solubility of carbon in austenite, carbides precipitate at the grain boundaries and increases in size. After water toughening, large microscopic porosity is left at grain boundaries, but in order to completely eliminate The silicon content in the steel is controlled to be 0.4-0.6%, and the silicon content is higher than 0.8%. There is no obvious effect on the performance of the high-manganese steel.

One new type high manganese steel crusher hammer with tic cermet rod is a good substitute for high chromium cast iron complex crusher hammer. It solves the problem of easy to be broken with high hardness in high chromium crusher hammer, furthermore, the wear life could be increased -up to 3 times, delivering fewer change-outs, more up time ,and lower maintenance costs. The titanium carbide columns provide structural strength to the hammer while the manganese or wear alloy give the hammer the flexibility to handle the impact. Both alloys work together to lengthen the overall wear life of the wear part.

cone crusher concave mantle with tic cermets rod

Click below link ,you will find details of workshop:

 

 please contact us to get FREE sample:

Changsha Langfeng Metallic Material Co., Ltd.

24 hours on line We-Chat & WhatsApp:

Rachel Chau: +86-15084863965

Tel: +86-731-86880480

E-mail: sales@langfengmaterials.com

 

Be the first to comment on "silicon content in high Mn castings"

Leave a comment

Your email address will not be published.


*